Steel composition
– Carbon: 0,97
– Chromium: 0,05
– Silicon: 0,23
– Manganese: 0,22
– Nickel: 0,03
– Phosphorous: 0,007
– Sulphurus: 0,008
– Copper: 0,11
Blade resistance Not inferior to 700HV (according to Vicker’s text)
Sterilization Gamma rays. Minimum dose: 25kGy (2,5M RADS)
Blades Two aluminium 0,08mm thick films welded together with a paper foil inside. Box of 100 blades with polythene film.
SRS110/18 type n.18
SRS110/20 type n.20
SRS110/21 type n.21
SRS110/22 type n.22
SRS110/23 type n.23
SRS110/24 type n.24
Steel composition
– Carbon: 0,97
– Chromium: 0,05
– Silicon: 0,23
– Manganese: 0,22
– Nickel: 0,03
– Phosphorous: 0,007
– Sulphurus: 0,008
– Copper: 0,11